Foundry2023

Q4 OES Controls CE and Nodularity of Ductile Iron

Q4 OES reads 18 elements including C, Si and Mg in 30 s at the furnace; CE held at 4.3±0.05% with nodularity above 90%, cutting composition-related scrap from 3.1% to 0.9%.

Company
A ductile iron foundry, C. China
Address
Luoyang, Henan
Q4 OES Controls CE and Nodularity of Ductile Iron
4.3±0.05%CE window
0.9%Composition scrap

QT500-7 ductile iron castings were tuned with a thermal-analysis cup and experience-based Mg additions. CE drifted ±0.15%, nodularity was unstable, and shrinkage or graphite flotation from composition swings caused 3.1% scrap.

Solution: a Q4 OES at the pouring furnace. After chill sampling, it reports 18 elements (C, Si, Mn, P, S, Mg, Cu) in 30 seconds, computes CE=C+Si/3 instantly, and alarms residual Mg outside the 0.035-0.055% window.

Results: CE tightened to 4.3±0.05% with 96% of batches in the Mg window; metallographic nodularity holds above 90% (grade 1-2 per GB/T 9441). Composition scrap fell to 0.9%, recovering about 1.8 million yuan of losses a year.

⇄0CompareProduct comparison