Stylus Qualification: Reference-Sphere Measurement and Tip Diameter Error

Qualification solves effective tip diameter and position on a reference sphere; an effective diameter off by more than 1 μm demands investigation.

华旋光电技术部
Stylus Qualification: Reference-Sphere Measurement and Tip Diameter Error

What qualification solves

Stylus qualification measures a reference sphere of known diameter — ceramic or ruby, roundness within 0.5 μm, diameter uncertainty within 0.5 μm — with a defined point pattern, typically 12-25 points in three or four tiers. The software solves two things: the effective ball diameter, the nominal value corrected for directional pre-travel of the trigger, and the ball-center position relative to the probe head reference. Every leg of a star stylus is qualified separately, and later stylus changes are stitched by the qualified positions.

Reading the report

Three key numbers: effective diameter within 1 μm of nominal — larger deviations point to a dirty sphere, a loose stylus or abnormal triggering; form error of the fitted sphere within 1-2 μm, reflecting probe repeatability; positional repeatability across repeated qualifications within 1 μm. Large form error often means excessive probing force bending a long thin stylus — a 100 mm needle bends several microns at standard force, so slow down or go stiffer.

Qualification strategy

Qualify the reference stylus on the sphere first, then link all other styli to the same sphere for a unified coordinate system. Keep the sphere fixed in the usual working area; moving it forces relinking of every stylus. Qualify every used A/B head angle: each head rotation shifts the ball position, and calling an unqualified angle errors out or injects position bias.

Interval and triggers

Qualify at the start of each shift as routine, and immediately after any crash, stylus change, head disassembly, ambient swing beyond 2 °C, or machine relocation. For intermediate checks, re-measure the reference sphere diameter: the indication should agree with the certificate within one third of the machine MPE, otherwise the qualification chain or machine state is suspect. Archive qualification data with dates — auditors always check traceability-chain completeness.