News0 views

CHWES launches HMAS-UHT1700CM, a 1600 °C hot hardness tester

For ceramics, refractory metals and thermal barrier coatings: 400–1600 °C, vacuum to 10⁻³ Pa, independent indenter heating.

华旋光电编辑部
CHWES launches HMAS-UHT1700CM, a 1600 °C hot hardness tester

In March 2026 CHWES launched the HMAS-UHT1700CM in Shanghai. Covering 400–1600 °C at ≤10⁻³ Pa with independent indenter and specimen heating, it holds ±5 °C uniformity and removes the oxidation and thermal drift that scatter high-temperature hardness data.

Unlike the previous generation, the UHT1700CM measures indentations directly with a high-temperature CCD, so specimens need not cool before measurement and shrinkage bias disappears. Software programs automatic gradients of up to 20 points through a case.

First units went to aero-materials institutes in Xi’an and Beijing for single-crystal blade and thermal-barrier coating evaluation.

⇄0VergleichTechnischer Vergleich