Dây cáp thép2024

Thử lực đứt toàn sợi cáp và kết nối dữ liệu

WAW-1000D 1000 kN thử đứt cáp theo GB/T 8358, sai số ±0,5%.

Công ty
Nhà máy cáp thép, Bắc Trung Quốc
Địa chỉ
Thiên Tân
Thử lực đứt toàn sợi cáp và kết nối dữ liệu
1000 kNDải đo
14 天 → 2 天Thời gian thử

The mill makes important-use wire rope of 16-32 mm diameter requiring full-rope breaking tests to GB/T 8358. Its 600 kN machine lacked capacity, so large ropes went to a third-party lab with a two-week turnaround and high fees.

Solution: a WAW-1000D servo-hydraulic universal testing machine, 1000 kN class 0.5. Both ends of the specimen are cast into zinc-alloy sockets and held in wedge grips; the loading rate is controlled within the standard range and the software captures the breaking peak with automatic judgement.

Result: a 28 mm rope broke at 512 kN, 106% of its minimum breaking force; the machine passed JJG 139 verification at class 0.5 with indication error within ±0.5%, and data upload to the group quality platform is automatic.

Benefit: all breaking tests are now in-house, lot turnaround fell from two weeks to two days, saving about CNY 300,000 a year in outsourcing fees.