Новости316 просмотров

CHWES и технический вуз Юго-Западного Китая открыли учебную базу металлографии

Учебная база оснащена полной линией пробоподготовки; первые 48 слушателей прошли аттестацию.

华旋光电编辑部
CHWES и технический вуз Юго-Западного Китая открыли учебную базу металлографии

About the base

The metallography training base, co-built with the materials analysis and testing center of a southwest university of technology, was officially inaugurated. It runs a complete preparation line — HXZDQ precision cutters, HXQ hot mounting presses and the HXZMP-3000 automatic grinding-polishing system — plus MMAS metallurgical microscopes with image-analysis software for result evaluation.

First training course

The first two-week course trained 48 participants, including 22 quality inspectors from industry and 26 graduate students. The practical assessment requires each trainee to prepare a quenched-steel specimen through the full workflow and rate grain size per GB/T 6394 within half a grade of the reference value; the pass rate reached 91.7 percent.

What follows

The base will run quarterly courses and add two modules on SEM sample preparation and failure analysis. Resident company application engineers teach with cases drawn from anonymized industrial data. The base also accepts commissioned sample preparation and testing from surrounding small and medium manufacturers, serving both teaching and the community.