SMAS-12 Stereo Microscope (单)

Stereo Microscope · 单

型番SMAS-12
  • 目镜WF10X(Φ20mm)
  • 物镜0.7X~4.5X
  • 放大倍数7X~45X
  • 视场范围Φ28.5~Φ4.5

By submitting you agree to our privacy policy.

01

製品概要

SMAS-12体视显微镜测量分析系统是将传统的光学显微镜与计算机通过光电转换有机的结合在一起,不仅可以在目镜上作显微观察,还能在计算机显示屏幕上观察图像,并能将所需要的图片进行编辑、保存和打印,同时还可以对被测工件的数据进行处理分析等。SMAS-12体视显微镜测量分析系统配备了研润自主研发的SMAS测量分析系统以及MOS高端光学系统。
SMAS-12体视显微镜测量分析系统可广泛应用于文教科研,农林地质,电子精密机械等行业和部门。
一、机械主机技术特点:
1、双目观察镜筒45°角倾斜,左右视度可调整。
2、WF10X广角目镜,视场范围可达20mm;
3、物镜从0.7~4.5X连续变倍。选配的附加镜头可以达到0.35X~9X;
4、可以选配环形LED和荧光照明光源;
二、技术参数:
目镜:WF10X(Φ20mm);
物镜:0.7X~4.5X;
放大倍数:7X~45X;
视场范围:Φ28.5~Φ4.5;
工作距离:88mm;
升降行程:25mm≤H<265mm;可选配挂壁式主机25mm≤H<130mm;
底座尺寸:215X160X60mm;
反射照明(上光源):12V,10W带反光杯卤素灯亮度可调;
三、标准配置:
1、SMAS控制系统;
2、笔记本电脑;
3、CCD;
4、1X适配镜;
5、主机;
6、目镜及物镜;
四、选配件:
目镜:
广角目镜 WF10X(Φ22mm);
广角目镜 WF15X(Φ15mm);
广角目镜 WF20X(Φ12mm);
广角目镜 WF25X(Φ9mm);
分划广角目镜10X(Φ20mm),格值0.1mm/格;
分划广角目镜10X(Φ22mm),格值0.1mm/格;
附加物镜:
0.5X,工作距离:137mm;
0.75X,工作距离:103mm;
1X,工作距离:88mm;
1.5X,工作距离:48mm;
2X,工作距离:29mm;
照明:
8W/90~265V,环形LED照明器工作距离35~200mm;
5W,110V/220V 荧光灯环形照明器;
五、软件功能:
1、实时图像、实时测量,具备线、线段、平行线、角度、圆形、椭圆、多边形、矩形等测试工具。
2、图像拼接功能,具备图像扫描后拼接功能,方便大尺寸工件的测试。
3、选配自动工作台后,具备动态图像拼接和测量功能。
4、具备各种报告输出功能。
5、具备定倍打印功能。

SMAS-12 Stereo Microscope (单) supplied by CHWES. 6 key specifications available on request.

02

仕様

目镜WF10X(Φ20mm)
物镜0.7X~4.5X
放大倍数7X~45X
视场范围Φ28.5~Φ4.5
工作距离88mm
升降行程25mm≤H<265mm;可

* Generated by rule engine over the product database; for pre-selection only.

03

測定原理

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

規格

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

選定ガイド

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

試験方法

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0比較仕様比較