FM-400 Metallurgical Microscope (无限远)

Metallurgical Microscope · 无限远

型番FM-400
  • 光学放大倍数40~1000X
  • 目镜大视野 WF10X(Φ20mm)
  • 无限远平场消色差物镜PL4X/0.;10X/0.;40X/0.65(弹簧)、100X/1.25(弹簧、油)
  • 荧光物镜FL25X/0.;40X/1.0(弹簧、甘油)

By submitting you agree to our privacy policy.

01

製品概要

FM-400正置无限远落射荧光显微镜采用优良的无限远光学系统与模块化功能设计理念,可提供出色的光学品质与操作性能,配置无放大率色差的无限远平场消色差荧光物镜和大视野目镜,光学系统成像清晰、明亮,视野广阔。符合人机工程学要求的理想设计,采用低位调焦手轮与内向式物镜转换器,使操作过程中更加舒适与轻松。可进行荧光显微术和透射明视场观察. 适用于生物制药,医学检测、疾病预防等领域。
一、技术特点:
1、铰链式双目观察镜筒,镜筒30度倾斜;大视野平场目镜,视场范围20mm;
2、转盘式落射荧光照明系统可提供UV、V、B、G四种荧光激发组,内置可表示视场光阑,视场光阑中心可调;
3、透射照明系统:适用于明视场观察和相衬观察,并且带有视场光栏集光器;
二、技术参数:
光学放大倍数:40~1000X;
目镜:大视野 WF10X(Φ20mm);
无限远平场消色差物镜PL:4X/0.10、10X/0.25、40X/0.65(弹簧)、100X/1.25(弹簧、油);
荧光物镜FL:25X/0.65、40X/1.0(弹簧、甘油);
目镜筒:三目镜,倾斜30度;
调焦机构:粗微动同轴,粗动松紧可调,带锁紧和限位装置,微动格值:2μm;
转换器:四孔(内向式滚珠内定位);
载物台:210*140mm,移动范围75*50mm;
阿贝聚光镜:N.A.1.25;
滤色片:蓝滤色片、磨砂玻璃;
集光器:卤素灯适用;
光源:6V20W卤素灯,亮度可调;
落射荧光照明:100W高压汞灯、电源箱110V/220V可选;
激发滤色片组:
蓝绿激发滤色片组:B蓝激发波长:450~490nm、发射波长:515nm;G绿激发波长:495~555nm、发射波长:595nm;
紫外、紫激发滤色片组:UV紫外激发波长:320~380nm、发射波长:435nm;V紫激发波长:380~415nm、发射波长:475nm;
三、选配件:
目镜:10X分划广角目镜(Φ20mm),格值0.1mm/格、大视野WF16X(Φ11mm);
物镜:无限远平场消色差物镜PL20X/0.4;
滤色片:绿、黄滤色片;
目镜筒:双目镜筒;
转换器:五孔;
100W宽电压恒功率荧光电源箱,带计时器;
落射荧光装置:紫外UV激发光波段320~380nm、紫V激发光波段380~415nm;
相衬目镜:对中望远镜;
无限远相衬平场消色差物镜PHP:10X/0.25、20X/0.40、40X/0.65(弹簧)、100X/1.25(弹簧、油);
转盘式相衬聚光镜:PH-I;
转盘式相衬聚光镜:PH-II;
插板式相衬聚光镜;
拉板式相衬聚光镜;
CCD适配镜:0.4X、0.5X、1X、0.5X带分划尺,格值0.1mm/格;
USB/VIDEO摄影接口;
数码相机接口;

FM-400 Metallurgical Microscope (无限远) supplied by CHWES. 17 key specifications available on request.

02

仕様

光学放大倍数40~1000X
目镜大视野 WF10X(Φ20mm)
无限远平场消色差物镜PL4X/0.;10X/0.;40X/0.65(弹簧)、100X/1.25(弹簧、油)
荧光物镜FL25X/0.;40X/1.0(弹簧、甘油)
目镜筒三目镜,倾斜30度
调焦机构粗微动同轴,粗动松紧可调,带锁紧和限位装置,微动格值:2μm
转换器四孔(内向式滚珠内定位)
载物台210*140mm,移动范围75*50mm
阿贝聚光镜N.A.1.25
滤色片蓝滤色片、磨砂玻璃
集光器卤素灯适用
光源6V20W卤素灯,亮度可调
落射荧光照明100W高压汞灯、电源箱110V/220V可选
蓝绿激发滤色片组B蓝激发波长:450~490nm、发射波长:515nm
G绿激发波长495~555nm、发射波长:595nm
紫外、紫激发滤色片组UV紫外激发波长:320~380nm、发射波长:435nm
V紫激发波长380~415nm、发射波长:475nm

* Generated by rule engine over the product database; for pre-selection only.

03

測定原理

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

規格

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

選定ガイド

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

試験方法

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.