HOT
BID-600 · 2026-11-17 · +86 21 5748 2007
BID-600 Biological Microscope
Biological Microscope
- 光学放大倍数50X~400X
- 机械筒长∞
- 物镜共轭距离∞
- 目镜大视野无色差SWF10X(Φ22mm)、对中目镜
By submitting you agree to our privacy policy.
製品概要
BID-600倒置透射微分干涉相衬生物显微镜是一种多功能新型光学显微镜,采用优良的无限远光学系统,可提供出色的光学性能。紧凑稳定的高刚性主体,充分体现了显微操作的防振要求。可拆装机械式载物台,采用同轴无齿轮、齿条传动系统,使传动更平稳与安全。旋转摆入摆出式聚光系统,配置透射式微分干涉相衬装置,以实现透射微分干涉相衬等显微观察功能,模块化设计使功能置换十分方便。本仪器适用于对透明组织的显微观察,应用于科研院所、高等院校、医疗卫生、检验检疫、农牧乳业等部门。
透射式微分干涉相衬观察适用于观察透明或半透明样品阻止,配置10X、20X微分干涉相衬物镜,在线性偏振光正交状态下,通过DIC分束棱镜,将偏振光分束成0光与E光,并通过样品组织时产生微小光程差,当0光和E光经过DIC复合棱镜时进行复合,并在物镜的后焦平面上发生干涉,行程干涉图样,然后通过检偏镜得到对比度较高和立体感较强的显微图像。
一、性能特点:
1、铰链式双目观察镜筒,镜筒45度倾斜;
2、高品质透明玻璃载物台板,很好降低载物台受热变形影响,物镜转换过程清晰可见;
3、高强度同轴挠性钢丝传动,极限位置自动保护功能,配备三种不同培养皿托板,适用于不同培养皿观察;
4、一体化照明系统,可对光源进行空间调整,有效控制照明装置的表面温度;
5、大视野目镜,视场范围直径22mm;
6、旋转摆入摆出式聚光系统,可对高培养迷你或圆筒状烧瓶进行无沾染培养细胞观察;
7、后置式摄影摄像接口设计,摄影摄像不干扰目镜观察;100%通光适合低照度的显微摄影摄像。
二、技术参数:
光学放大倍数:50X~400X;
机械筒长:∞;
物镜共轭距离:∞;
目镜:大视野无色差SWF10X(Φ22mm)、对中目镜;
目镜:铰链双目,观察角度为45度,瞳距为53~75mm;
目镜接口:Ф30mm;
齐焦距离:10mm;
微分干涉相衬物镜:5X/0.12\工作距离18.2mm,10X/0.25\20.2mm,20X/0.35\6mm;
明视场物镜(盖玻片厚度1.2mm):40X/0.6\工作距离3.5mm;
相位相衬物镜(盖玻片厚度1.2mm):10X/0.25\工作距离4.3mm;
转换器:五孔转换器;
聚光镜:工作距离55mm,数值孔径0.30;
载物台:移动范围77mm(纵向)*134.5mm(横向),移动尺可拆卸;
调焦机构:粗微动同轴调节,微动手轮格植:0.002mm;
培养皿托板一:86mm(宽)X129.5mm(长),可适配圆形培养皿Ф87.5mm;
培养皿托板二:34mm(宽)X77.5mm(长),可适配圆形培养皿Ф68.5mm;
培养皿托板三:57mm(宽)X82mm(长);
光源:5W/白光(色温5000~5500K)LED照明器,输入电压3.9~4.0V;
BID-600 Biological Microscope supplied by CHWES. 17 key specifications available on request.
仕様
| 光学放大倍数 | 50X~400X |
|---|---|
| 机械筒长 | ∞ |
| 物镜共轭距离 | ∞ |
| 目镜 | 大视野无色差SWF10X(Φ22mm)、对中目镜 |
| 目镜接口 | Ф30mm |
| 齐焦距离 | 10mm |
| 微分干涉相衬物镜 | 5X/0.12\工作距离18.2mm,10X/0.25\20.2mm,20X/0.35\6mm |
| 明视场物镜(盖玻片厚度1.2mm) | 40X/0.6\工作距离3.5mm |
| 相位相衬物镜(盖玻片厚度1.2mm) | 10X/0.25\工作距离4.3mm |
| 转换器 | 五孔转换器 |
| 聚光镜 | 工作距离55mm,数值孔径0.30 |
| 载物台 | 移动范围77mm(纵向)*134.5mm(横向),移动尺可拆卸 |
| 调焦机构 | 粗微动同轴调节,微动手轮格植:0.002mm |
| 培养皿托板一 | 86mm(宽)X129.5mm(长),可适配圆形培养皿Ф87.5mm |
| 培养皿托板二 | 34mm(宽)X77.5mm(长),可适配圆形培养皿Ф68.5mm |
| 培养皿托板三 | 57mm(宽)X82mm(长) |
| 光源 | 5W/白光(色温5000~5500K)LED照明器,输入电压3.9~4.0V |
* Generated by rule engine over the product database; for pre-selection only.
測定原理
The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.
- Bright field for routine microstructure, inclusions and decarburised layers.
- Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
- Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
- DIC converts tiny height differences into contrast, ideal for polished, unetched samples.
Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.
Process animation
- Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
- Illumination and focus: select BF/DF/POL/DIC and focus.
- Image capture: trinocular port, 1× camera adapter, white balance.
- Scale calibration: calibrate µm per pixel with a stage micrometer.
- Measurement: grain size, case depth, coating thickness, inclusion rating.
Calculation & formulas
1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.
2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.
3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.
4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).
5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.
規格
| Standard | Title | Scope |
|---|---|---|
| GB/T 13298-2015 | Metallic materials — examination of microstructure | Microstructure rating |
| GB/T 6394-2017 | Determination of average grain size | Grain size |
| ASTM E3-11 | Guide for metallographic specimen preparation | Preparation |
| ASTM E112 | Determining average grain size | Grain size |
| ISO 643 | Steels — micrographic determination of grain size | Grain size |
Export projects often require dual GB and ASTM reports; the software ships both rating charts.
選定ガイド
1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.
2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.
3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.
4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.
5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.
6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.
| Series | Type | Typical task | Recommended setup |
|---|---|---|---|
| HX-4A / HX-4B | Upright metallurgical | Routine structure, case depth | 5×/10×/40× + 5 MP camera |
| HX-G2A / G2B | Inverted | Batch samples, no re-mounting | Brightfield + simple polariser |
| HX-G3A | Trinocular inverted | Case depth, rating, reports | Camera + analysis software |
| HX-G4C / G5A | Research inverted | Darkfield/polarised/DIC | Semi-apochromat + motorised stage |
| HX-ZG7 / XSZ-146 | Stereo | Fracture, solder, low-mag locating | Zoom + ring light |
Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.
試験方法
Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.
Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.
Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.
Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.
Industry applications
- Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
- Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
- Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
- Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
- Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
- Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
- Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
- Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.