News582 views

CHWES Delivers Multiple Hot Hardness Testers to Overseas Customers, Passing Acceptance

Three IMAS hot hardness testers shipped to Southeast Asia and the Middle East, passing on-site acceptance on vacuum, temperature uniformity and hardness indication.

华旋光电编辑部
CHWES Delivers Multiple Hot Hardness Testers to Overseas Customers, Passing Acceptance

Delivery overview

Three IMAS-series hot hardness testers were recently delivered overseas: two IMAS-HT1500CM to a materials research institute in Southeast Asia and one IMAS-UHT1700CM to an energy-equipment laboratory in the Middle East. After sea freight arrival, two engineer teams handled installation and commissioning, and all units passed the customers' on-site acceptance.

Acceptance data

Acceptance followed the technical agreement item by item: ultimate vacuum better than 5×10⁻³ Pa and static pressure-rise rate below 5 Pa·L/s; working-zone temperature uniformity of ±2 °C across a nine-point survey at the 1000 °C hold; hardness indication verified with reference blocks, within ±3 percent relative error and 2.1 percent repeatability at 800 °C. The Middle East UHT1700CM additionally completed a 1600 °C no-load ramp and indenter temperature-equalization verification, meeting the agreed figures.

Service assurance

Overseas customers receive English operation training, remote diagnostics access and a first-year spares kit covering indenters, heater elements and seals. Both sites are now in trial operation with equipment data linked to the company's remote monitoring platform. This delivery produced a complete installation-and-acceptance process template for volume overseas shipments of the hot product line.

⇄0比較仕様比較